Welcome to Metal Mine! Today is Share:
×

扫码分享

Modern Mining ›› 2025, Vol. 41 ›› Issue (06): 152-154,159.

Previous Articles     Next Articles

Experimental Study on Mixed Separation of a Zinc-Molybdenum Ore in Hebei

  

  1. Laiyuan Nonferrous Metals Co.,Ltd.,Hebei Iron and Steel Group
  • Online:2025-06-25 Published:2025-08-04

Abstract: The contents of zinc and molybdenum in a zinc-molybdenum ore dressing plant in Hebei Province are 0.85% and 0.12%,respectively. In view of the low recovery index of molybdenum and zinc in the original on-site process flow,zinc-molybdenum mixed flotation and separation process is proposed to treat the ore. The results show that under the condition of grinding fineness of - 0.074 mm accounting for 65%,with CuSO4 as activator,butyl xanthate and kerosene as collector,via one roughing two scavenging Mo-Zn mixed flotation,first stage concentrate was reground to - 0.043 mm accounting for 82%. After two stages of blank cleaning,the concentrate is treated with CuSO4 as activator,ZnSO4 + Na2SO3 as inhibitor and sodium silicate as dispersant. After one roughing,five cleaning and one scavenging cleaning separa⁃ tion,the molybdenum concentrate with molybdenum grade of 38.65% and recovery of 75.05% is finally ob⁃ tained. The zinc grade of zinc concentrate is 45.68% and the recovery rate is 73.09%. The zinc-molybdenum mixed flotation and separation process significantly improves the metal recovery rate and concentrate quali⁃ ty,which can provide a reference for the separation of similar ores.

Key words: zinc-molybdenum ore, mixed flotation, recovery rate, mixed inhibitor