摘要: 为高效回收大红山铁矿二段强磁精矿中的-0.045 mm粒级铁矿物,针对该粒级金属分 布率超过 75%、原摇床工艺分选效果差、金属流失严重的问题,进行了 Slon 连续离心选矿机半工业 试验、参数优化及工业应用研究。试验结果表明:在工业最优操作参数给矿浓度20%~25%、给矿时 间 90~110 s、漂洗时间 5~25 s、卸矿时间 8~15 s、转鼓转速 180 r/min、冲洗水压力 0.3~0.4 MPa 的 条件下,当给矿 TFe 品位为 42%~48% 时,工业连续生产获得的精矿铁品位为 52%~58%,铁回收 率为 55%~66%;采用强磁粗选+离心机精选+摇床扫选联合流程,总精矿铁品位由原工艺的 62.37% 提升至 63.50%,年净增经济效益约 6 293万元,静态投资回收期约 5.7个月,该联合工艺绿色 环保且应用效果稳定可靠,可有效解决微细粒级铁矿物高效回收难题,经济效益显著。

关键词: Slon连续离心选矿机, 微细粒赤铁矿, 回收率, 工艺参数优化, 工业应用

Abstract: In order to efficiently recover the -0.045 mm iron minerals in the second-stage high-in⁃ tensity magnetic concentrate of Dahongshan Iron Mine, the semi-industrial test, parameter optimization and industrial application of SLon continuous centrifugal concentrator are carried out to solve the problems of metal distribution rate exceeding 75%, poor separation effect and serious metal loss in the original shaking table process.The test results show that under the conditions of industrial optimal operating parameters of ore feeding concentration of 20%~25%, ore feeding time of 90~110 s, rinsing time of 5~25 s, ore unloading time of 8~15 s, drum speed of 180 r/min, and flushing water pressure of 0.3~0.4 MPa, when the TFe grade of ore feeding is 42%~48%, the iron grade of concentrate obtained by industrial continuous production is 52%~58%, and the iron recovery rate is 55%~66%. The combined process of high-intensity magnetic roughing + centrifuge cleaning + shaker scavenging is adopted. The iron grade of the total concentrate is in⁃ creased from 62.37% of the original process to 63.50%. The annual net economic benefit is about 62.93 million yuan, and the static investment recovery period is about 5.7 months. The combined process is green and environmentally friendly, and the application effect is stable and reliable. It can effectively solve the problem of efficient recovery of fine-grained iron minerals, and the economic benefits are remarkable.

Key words: SLon continuous centrifugal concentrator, micro-fine hematite, recovery rate, process pa? rameter optimization, industrial application