欢迎访问《现代矿业》杂志官方网站,今天是 分享到:
×

扫码分享

现代矿业 ›› 2023, Vol. 39 ›› Issue (02): 16-18.

• 铁矿石加工与铁回收专栏 • 上一篇    下一篇

河南某铁铜矿石优先浮铜尾矿弱磁选铁试验

赵凯1 张春艳1 赵永利1 王新宇2 张东亮3 张森森4 石俊超2   

  1. 1. 河南省有色金属地质矿产局第五地质大队;2. 河南有色金源实业有限公司; 3. 中南大学地球科学与信息学院;4. 河南省地质研究院
  • 出版日期:2023-02-25 发布日期:2023-05-09
  • 基金资助:
    河南省地质勘查基金项目(编号:05035);河南省有色金属地质矿产局2022 年重点项目(编号:zd2022-01)

Experimental Study on Low Intensity Magnetic Separation of Preferential Copper Flotation Tailings from an Iron-Copper Deposit in Henan

ZHAO Kai1 ZHANG Chunyan1 ZHAO Yongli1 WANG Xinyu2 ZHANG Dongliang3 ZHANG Sensen4 SHI Junchao2#br#   

  1. 1. The Fifth Branch Team of Henan Geological Bureau of Non-ferrous Metal and Mineral Resources; 2. Henan Non-ferrous Jinyuan Industrial Co.,Ltd.;3. School of Earth Sciences and Information,Central South University;4.Henan Institute of Geology
  • Online:2023-02-25 Published:2023-05-09

摘要: 河南某铁铜矿石结构构造及矿物组成均较简单,有用矿物磁铁矿和黄铜矿的粒度均 较粗。为了确定2 粗3 精2 扫闭路优先浮铜尾矿弱磁选选铁的合理工艺流程,开展了直接1 粗1 精 弱磁选、弱磁粗选精矿磨矿后弱磁精选、先磨矿后1 粗1 精弱磁选3 种工艺选铁试验。结果表明, 弱磁粗选精矿磨矿后弱磁精选工艺效果最佳,在再磨细度为-0.074 mm 90%、弱磁粗选和弱磁精选 磁场强度分别为95.54 kA/m和67.58 kA/m情况下,可获得铁品位65.50%、回收率53.53%的铁精矿。

关键词: 铁精矿, 磁选, 磁铁矿, 黄铁矿

Abstract: The structure and mineral composition of an iron-copper deposit in Henan are both simple. The main minerals are magnetite and chalcopyrite,which are coarse grained. In order to determine the technological processing reasonability of low intensity magnetic separation of preferential copper flotation tailings by the closed-circuit process of two roughing,three cleaning,two scavenging,three kinds of iron separation ways have been tested including one roughing one cleaning low intensity magnetic separation for iron,low intensity magnetic cleaning separation using low intensity magnetic rough separation concentrate after grinding,one roughing one cleaning low intensity magnetic separation after grinding. The results showed that the ideal process is low intensity magnetic cleaning separation using low intensity magnetic rough separation concentrate after grinding. When the regrinding fineness reached 90% passing 0.074 mm, the iron concentrate is iron grade of 65.50% and recovery rate of 53.53% with the low intensity magnetic rough separation of 95.54 kA/m and the low intensity magnetic cleaning separation of 67.58 kA/m.

Key words: iron concentrate, magnetic separation, magnetite, pyrite