安徽某磁铁矿脱泥抛尾选矿工艺研究

蒋丰祥 胡城 揣新 李伟 杨俊 张亚坤 杨顺   

  1. 安徽马钢矿业资源集团南山矿业有限公司
  • 出版日期:2023-01-25 发布日期:2023-05-12

Study on Mineral Processing Technology of Desliming and Discarding Tailings of a Magnetite Ore in Anhui Province

JIANG Fengxiang Hu Cheng CHUAI Xin LI Wei YANG Jun ZHANG Yakun YANG Shun   

  1. Nanshan Mining Co.,Ltd.,Anhui Masteel Mining Resources Group
  • Online:2023-01-25 Published:2023-05-12

摘要: 安徽某磁铁矿为解决生产流程堵塞难题,针对含泥量大的问题,对中碎前预先筛分 筛下矿石进行了脱泥抛尾试验。试验结果表明:①原矿采用干式磁选工艺,可抛弃产率48.37%、 全铁品位13.12%、磁性铁品位4.62% 的尾矿,磁性铁回收率79.91%;②对原矿中粒75~20 mm、 20~0 mm 物料分别采用干式磁选工艺,可抛弃产率41.80%、全铁品位11.78%、磁性铁品位0.64% 的尾矿,可获得全铁品位18.37%、磁性铁品位8.81%的综合铁精矿;③原矿采用高压辊磨+湿式磁 选工艺,可抛弃产率37.75%、全铁品位9.35%、磁性铁品位0.33%的尾矿,精矿品位提高至22.89%, 磁性铁回收率达98.89%,湿式预选指标较优。

关键词: 脱泥抛尾, 磁铁矿, 预选

Abstract: In order to solve the problem of blockage in the production process of a magnetite mine in Anhui Province,aiming at the problem of large mud content,the desliming and discarding test was carried out on the ore under pre-screening and screening before medium crushing. The results show that: ① The tailings with yield of 48.37%,total iron grade of 13.12% and magnetic iron grade of 4.62% can be discarded by dry magnetic separation process,and the recovery rate of magnetic iron is 79.91%. ② The tailings with yield of 41.80%,total iron grade of 11.78% and magnetic iron grade of 0.64% can be discarded by dry magnetic separation process for 75~20 mm and 20~0 mm raw ore,and comprehensive iron concentrate with total iron grade of 18.37% and magnetic iron grade of 8.81% can be obtained. ③The tailings with yield of 37.75%,total iron grade of 9.35% and magnetic iron grade of 0.33% can be discarded by using high pressure roller mill + wet magnetic separation process. The concentrate grade is increased to 22.89%,the recovery rate of magnetic iron is 98.89%,and the wet preconcentration index is better.

Key words: desliming and discavding tailings, magnetite, preselection