现代矿业 ›› 2012, Vol. 28 ›› Issue (12): 25-28.
• 采选工程 • 上一篇 下一篇
刘卫,罗良飞,杨备
出版日期:
发布日期:
Liu Wei,Luo Liangfei,Yang Bei
Online:
Published:
摘要: 针对云南某低品位磁铁矿工艺矿物学特点,通过试验确定采用磁滑轮干式预选—3段阶磨—5段弱磁选工艺流程,对原矿TFe品位仅为19.68%(其中磁性铁品位仅为7.57%)的单一原生磁铁矿进行了研究,试验获得了铁精矿TFe品位为68.07%、回收率为45.14%(对原矿37.16%)的较好技术指标。
关键词: 低品位磁铁矿, 干式预选, 阶段磨矿, 磁选
Abstract: In the light of the process mineralogy characteristics of a low-grade magnetite in Yunnan, the process of dry primary concentration with magnetic pulley-three-stage grinding-five-stage low intensity magnetic separation was determined by the tests to make research on single native magnetite with TFe grade of 19.68% (magnetic iron grade of only 7.57%). Finally, good technical indicators of iron concentrate with TFe grade of 68.07% and recovery of 45.14% (37.16% in raw ore) were obtained.
Key words: Low-grade magnetite, Dry primary concentration, Stage grinding, Magnetic separation
刘卫, 罗良飞, 杨备. 云南某低品位磁铁矿选矿试验[J]. 现代矿业, 2012, 28(12): 25-28.
LIU Wei, LUO Liang-Fei, YANG Bei. Beneficiation Tests of a Low-grade Magnetite of Yunnan[J]. Modern Mining, 2012, 28(12): 25-28.