The copper content of a copper-bearing pyrite in Jiangxi is 1.33%,of which copper oxide accounts for 15.79% and sulfur content is 32.24%. In order to develop and utilize the ore,a closed-circuit test was carried out with lime as pH regulator,APII as copper collector and butyl xanthate as sulfur collector under the grinding fineness of -0.074 mm accounting for 70%. The flotation indexes of copper concentrate with copper grade of 17.97%,copper recovery of 72.21%,gold grade of 4.69 g/t,silver grade of 160.53 g/t and sulfur concentrate with sulfur grade of 48.93% and sulfur recovery of 89.05% were obtained. The recov⁃ery and utilization of valuable metals in the ore are realized,which provides a basis for the efficient develop⁃ment and utilization of the ore.   

  1. 1.Jiangxi Jiangtong Yinzhushan Mining Co.,Ltd.;
    2.China Nerin Engineering Co.,Ltd.
  • Online:2024-06-17 Published:2024-08-07

Abstract:

The copper content of a copper-bearing pyrite in Jiangxi is 1.33%,of which copper oxide accounts for 15.79% and sulfur content is 32.24%. In order to develop and utilize the ore,a closed-circuit test was carried out with lime as pH regulator,APII as copper collector and butyl xanthate as sulfur collector under the grinding fineness of -0.074 mm accounting for 70%. The flotation indexes of copper concentrate with copper grade of 17.97%,copper recovery of 72.21%,gold grade of 4.69 g/t,silver grade of 160.53 g/t and sulfur concentrate with sulfur grade of 48.93% and sulfur recovery of 89.05% were obtained. The recov⁃ery and utilization of valuable metals in the ore are realized,which provides a basis for the efficient develop⁃ment and utilization of the ore.

Key words: