Welcome to Metal Mine! Today is Share:
×

扫码分享

Modern Mining ›› 2016, Vol. 32 ›› Issue (09): 73-77+93.

Previous Articles     Next Articles

Cobalt Sulfur Recovery from Vanadium-titanium-iron Concentrate

Wang Yong1,2   

  1. 1.Design and Research Institute of Pangang Group Mining Co., Ltd.;2.State Key Laboratory of Vanadium and Titanium Resources Comprehensive Utilization
  • Online:2016-09-20 Published:2016-11-14

Abstract: To comprehensive recovery of sulphur and cobalt from Panzhihua Mining Co., Ltd. production of vanadium-titanium-iron concentrate, based on the analysis of the mineralogy technological, flotation condition test, open flow experiment and the whole process experiment by the grinding method, magnetic separation and flotation method was conducted. Experimental results show that via grinding low intensity magnetic separation-magnetism sweep-one roughing three cleaning one scavenging sulfur flotation open process, sulfur-cobalt concentrate with 56.02% Fe, 30.02% S, 0.30% Co, sulfur and cobalt recovery of 16.411% and 6.15% was obtained, Desulfurization iron concentrate with iron grade of 5569%, sulfur grade of 0.284%;Recommended industrial test process is classification grinding-low intensity magnetic separation and magnetism sweep-one roughing three cleaning one scavenging sulfur flotation closed-circuit flotation coarse.

Key words: Vanadium-titanium-iron concentrate, Magnetic separation, Sulfur float, Sulfur-cobalt concentrate, Sulfur-cobalt recovery