某含砷金精矿生物预氧化浸金工艺试验

邹毅仁 于保强 马 帅   

  1. 中国恩菲工程技术有限公司
  • 出版日期:2026-09-25 发布日期:2026-10-10

Biological Pre-oxidation Gold Leaching Process Test of an Arsenic-containing Gold Concentrate

  1. China ENFI Engineering Corporation
  • Online:2026-09-25 Published:2026-10-10

摘要: 为实现含砷金精矿中金资源的高效回收,针对某含砷金精矿中金矿物被包裹、直接氰 化浸金效率低下的难题,开展了生物预氧化处理—氰化浸金工艺优化及浸出动力学特性研究。通过 调控磨矿细度、矿浆浓度、溶氧量及培养基用量等预氧化关键参数,破除砷、硫矿物对金颗粒的包裹 阻隔,系统考察氧化钙和氰化钠用量、矿浆浓度及浸出时间对金浸出效果的影响,并结合扫描电镜微 观表征与动力学拟合分析揭示提金强化机制。试验结果表明:最优生物预氧化条件下,金精矿中砷、 硫氧化率分别可达 82.95% 和 81.34%;对应的预氧化渣在适宜浸金参数下,金平均浸出率可达 92.03%,较原矿直接浸出金浸出率32.45%大幅提升。扫描微观形貌分析证实,生物预氧化可使矿物 表面生成大量孔隙与裂隙,有效改善浸金反应条件;动力学拟合结果表明,该金精矿浸出过程受化学 反应与内扩散双重控制,符合混合控制模型特征;该研究成果可为含砷难处理金精矿的高效开发利 用提供技术支撑。

关键词: 含砷金精矿, 生物预氧化, 氰化浸金, 反应动力学

Abstract: In order to realize the efficient recovery of gold resources in arsenic-containing gold con⁃ centrate,aiming at the problem that gold minerals in arsenic-containing gold concentrate are wrapped and the efficiency of direct cyanide leaching of gold is low,the process optimization and leaching kinetics char⁃ acteristics of biological pre-oxidation treatment-cyanide leaching of gold are studied.By adjusting the key parameters of pre-oxidation such as grinding fineness,pulp concentration,dissolved oxygen and medium dosage,the encapsulation barrier of arsenic and sulfur minerals to gold particles is broken. The effects of calcium oxide and sodium cyanide dosage,pulp concentration and leaching time on gold leaching are sys⁃ tematically investigated. The strengthening mechanism of gold extraction is revealed by scanning electron microscopy and kinetic fitting analysis.The results show that under the optimal biological pre-oxidation con⁃ ditions,the oxidation rates of arsenic and sulfur in gold concentrate can reach 82.95% and 81.34% respec⁃ tively. Under the appropriate leaching parameters,the average gold leaching rate of the corresponding pre�oxidized slag can reach 92.03%,which is greatly improved compared with the raw oredirect leaching gold leaching rate of 32.45%. Scanning micro-morphology analysis confirms that biological pre-oxidation can generate a large number of pores and cracks on the mineral surface,effectively improving the gold leaching reaction conditions.The results of kinetic fitting show that the leaching process of gold concentrate is con⁃ trolled by both chemical reaction and internal diffusion,which accords with the characteristics of mixed con⁃ trol model. The research results can provide technical support for the efficient development and utilization of arsenic-containing refractory gold concentrate.

Key words: arsenic-containing gold concentrate, biological pre-oxidation, cyanide leaching of gold