梅山铁矿铁精矿降硅选矿工艺试验

勾金玲,徐望华   

  1. 宝钢集团(南京)梅山矿业公司选矿厂
  • 出版日期:2013-07-15 发布日期:2013-08-22

Beneficiation Tests on Reduce Silicon of Iron Concentrate in Meishan Iron Plant

Gou Jinling,Xu Wanghua   

  1. Concentrator of BaoSteel Group (Shanghai) Meishan Mining Co. Ltd.
  • Online:2013-07-15 Published:2013-08-22

摘要: 为进一步满足冶炼对铁精矿质量的要求,梅山铁矿选矿厂需降低铁精矿中SiO2的含量。为此,对生产出的强磁精矿进行了正浮选和细筛—再磨强磁选2种工艺流程的降硅试验研究。试验结果表明:2种工艺都能有效降低总精矿中的SiO2含量至4%以下,虽回收率有所损失,但最终精矿的碱比明显提高,矿石的自熔性变好,建议对这2种工艺进行试验室扩大连续试验和工业试验,以为现场技术改造提供参考依据。

关键词: 铁精矿, 降硅, 正浮选, 细筛&mdash, 再磨强磁选工艺

Abstract: Reduce the content of SiO2 in iron ore concentrate become a necessity for Meishan iron ore, in order to well meet the smelting requirements of iron ore quality. Study was conducted with positive flotation and fine sieve-regrinding and strong magnetic process separately. The results showed that: both of the two process could ruduce the content of SiO2 to 4% in total concentrate, though recovery rate was lower, but the alkali ratio significantly increased, and the self-fluxing quality become better. Laboratory and industrial tests was suggested to continue, in order to provide reference basis for on-site process.

Key words: Iron concentrate, Reduce of silicon, Positive flotation, Fine sieve-regrinding and high intensity magnetic process