某锂矿尾泥综合回收利用技术研究

陈红康 赵 辉   

  1. 宜春国轩锂业工程研究院
  • 出版日期:2026-04-25 发布日期:2026-05-28

Research on Comprehensive Recovery and Utilization Technology for Tailings from a Lithium Ore 

CHEN Hongkang ZHAO Hui   

  1. Yichun Guoxuan Lithium Industry Engineering Research Institute
  • Online:2026-04-25 Published:2026-05-28

摘要: 针对某锂云母选矿厂尾泥胀库、消纳困难及资源浪费等问题,以该厂尾泥为研究对象, 在性质分析的基础上开展了综合回收利用技术研究。结果表明,尾泥Li₂O 品位为0 .33%,其中云母是 锂的主要载体矿物,分布率达94 .82%。通过系统研究磁选参数、捕收剂组合和抑制剂组合对细粒锂 云母回收的影响,确定了最优操作条件:采用刚毛介质、1.5 T 磁感应强度对尾泥浆料进行磁选预富 集,获得Li₂O 品位0 .68%、回收率78 .11%的磁选精矿,尾矿白度达56 .2。磁选精矿浮选时,选用椰油 胺与油酸钠的阴阳离子组合捕收剂(用量比1∶2,总用量500 g/t),在六偏磷酸钠与烤胶的组合抑制剂 体系下(用量比1∶2,总用量400 g/t),通过1 粗2 精1 扫闭路浮选流程,最终获得Li₂O 品位1 .62%、回收 率79 .56%的锂云母精矿,并得到白度56 .2%的细长石粉。该工艺有效实现了锂矿尾泥中锂资源的 高效回收,为尾泥的资源化利用提供了可靠的技术依据。

关键词: 锂矿尾泥, 磁选, 浮选, 综合回收

Abstract: Aiming at the problems of tailings expansion,difficult consumption and waste of resources in a lepidolite concentrator,the tailings of the plant were taken as the research object,and the comprehen⁃ sive recycling technology was studied on the basis of property analysis.The results show that the grade of Li2O in the tailings is 0.33%,in which mica is the main carrier mineral of lithium ,and the distribution rate is 94.82%.By systematically studying the effects of magnetic separation parameters ,collector combination and inhibitor combination on the recovery of fine-grained lepidolite ,the optimal operating conditions were determined.The magnetic separation pre-concentration of tailings slurry was carried out by using the bristle medium and 1.5 T magnetic induction intensity,and the magnetic concentrate with Li2O grade of 0.68%and recovery rate of 78.11%was obtained,and the whiteness of tailings reached 56.2.In the flotation of magnet⁃ ic separation concentrate,the combined collector of cocoylamine and sodium oleate(dosage ratio 1 ∶2,total dosage 500 g/t)was selected,and the combined inhibitor system of sodium hexametaphosphate and baking gum (dosage ratio 1 ∶2,total dosage 400 g/t)was used.Through the closed-circuit flotation process of one roughing,two cleaning and one scavenging,the lepidolite concentrate with Li2O grade of 1.62%and recov⁃ ery rate of 79.56%was finally obtained,and the feldspar powder with whiteness of 56.2%was obtained. The process effectively realizes the efficient recovery of lithium resources in lithium tailings ,and provides a reliable technical basis for the resource utilization of tailings.

Key words: lithium tailings, magnetic separation, flotation, comprehensive recovery