欢迎访问《现代矿业》杂志官方网站,今天是 分享到:
×

扫码分享

现代矿业 ›› 2026, Vol. 42 ›› Issue (02): 79-84,89.

• 矿物加工工程 • 上一篇    下一篇

酒钢焙烧磁选精矿工艺矿物学研究

董再蒸1,2,3 孙洪硕3 先佳宇1,2 刘 杰1,2   

  1. 1. 矿物加工科学与技术全国重点实验室;2. 东北大学资源与土木工程学院实验中心; 3. 酒泉钢铁(集团)有限责任公司
  • 出版日期:2026-02-25 发布日期:2026-03-11

Process Mineralogy Study on the Roasted Magnetic Separation Concentrate of JISCO

  1. 1. State Key Laboratory of Mineral Processing;2. Experimental Center,School of Resources and Civil Engineering,Northeastern University;3. Jiuquan Iron and Steel(Group)Co.,Ltd.
  • Online:2026-02-25 Published:2026-03-11

摘要: 以酒钢选矿厂悬浮焙烧—磁选工艺获得的三段焙烧磁选精矿为研究对象,综合运 用化学分析、光学显微观察、矿物自动分析、X 射线衍射(XRD)及红外光谱(FTIR)等表征手段,系 统分析了其工艺矿物学特性。结果表明:焙烧磁选精矿的铁品位为 53.62%,铁元素主要赋存于 磁铁矿及焙烧后菱铁矿中。磁/赤铁矿的单体解离率为 39.14%,整体呈现出细粒级分布广、嵌布 关系复杂的特点。石英作为主要脉石矿物,多以粒状集合体形式产出,并与铁矿物紧密共生。 在+0.038 mm 粒级中,铁矿物与石英形成复杂共生结构,阻碍了选矿药剂在矿物表面的有效吸附, 导致表面改性困难;而在-0.038 mm 粒级中,尽管铁矿物解离度较高,但超细颗粒因表面能增大而 易被浮选泡沫夹带,造成金属流失,影响分选指标。

关键词: 焙烧磁选精矿, 工艺矿物学, 解离

Abstract: Taking the third-stage magnetic separation concentrate obtained by the suspension roast⁃ ing-magnetic separation process in the concentrator of Jiuquan Iron and Steel Co.,Ltd. as the research ob⁃ ject,the process mineralogy characteristics were systematically analyzed by means of chemical analysis, optical microscopic observation,automatic mineral analysis,X-ray diffraction(XRD)and infrared spec⁃ troscopy(FTIR). The results show that the iron grade of the roasted magnetic concentrate is 53.62%,and the iron element mainly exists in magnetite and roasted siderite. The monomer dissociation rate of magne⁃ tite/hematite is 39.14%,which shows the characteristics of wide distribution of fine particles and complex embedding relationship. As the main gangue mineral,quartz is mostly produced in the form of granular ag⁃ gregates and is closely associated with iron minerals. In the +0.038 mm fraction,iron minerals and quartz form a complex symbiotic structure,which hinders the effective adsorption of beneficiation reagents on the mineral surface,resulting in difficult surface modification. In the −0.038 mm fraction,although the disso⁃ ciation degree of iron minerals is high,the ultrafine particles are easily entrained by flotation foam due to the increase of surface energy,resulting in metal loss and affecting the separation index.

Key words: roasted magnetic concentrate, process mineralogy, dissociation