欢迎访问《现代矿业》杂志官方网站,今天是 分享到:
×

扫码分享

现代矿业 ›› 2025, Vol. 41 ›› Issue (12): 115-119,124.

• 矿物加工工程 • 上一篇    下一篇

阴离子捕收剂RS强化高泥化铜钴矿浮选试验研究

高丹校1 曾 培1,2 李宋江3 张自旭1 邵 坤1 顾鹏飞1   

  1. 1. 华刚矿业股份有限公司;2. 中南大学资源加工与生物工程学院;3. 中铁资源集团有限公司
  • 出版日期:2025-12-25 发布日期:2026-01-23

Research on the Flotation Experiment of High Mud Copper-Cobalt Ore Using Anionic Collector RS

  1. 1. Huagang Mining Co., Ltd.;2. School of Mineral Processing and Bioengineering, Central South University;3. China Railway Resources Co.,Ltd.
  • Online:2025-12-25 Published:2026-01-23

摘要: 刚果(金)SICOMINES 高泥化铜钴矿原矿铜品位为 2.51%,钴品位为 0.246%,矿石泥 化严重,可选性较差,铜、钴浮选回收率不高。为强化高泥化铜钴矿选别,使用阴离子捕收剂 RS 进 行强化浮选。最终获得铜、钴品位分别为 4.05%、0.72%,铜、钴回收率分别为 4.10%、7.83% 的硫化 铜精矿,铜、钴品位分别为 10.16%、0.56%,铜、钴回收率分别为 71.05%、41.89% 的氧化铜精矿,铜、 钴品位分别为 1.41%、0.21%,铜、钴回收率分别为 8.00%、12.83% 的强化浮选精矿,硫化铜精矿、氧 化铜精矿和强化浮选精矿合计铜总回收率为 83.15%,钴总回收率为 62.55%,显著提高了高泥化铜 钴矿的资源利用率。

关键词: 高泥化铜钴矿, 阴离子捕收剂RS, 浮选

Abstract: The grade of copper and cobalt in high mud copper-cobalt ore from SICOMINES in Congo (DRC) is 2.51% and 0.246% respectively. The ore is seriously mudded, the washability is poor, and the flo‐ tation recovery rate of copper and cobalt is not high. In order to strengthen the separation of high-slime cop‐ per-cobalt ore, the anionic collector RS was used for enhanced flotation. Finally, a copper sulfide concen‐ trate with copper and cobalt grades of 4.05% and 0.72%, copper and cobalt recovery rates of 4.10% and 7.83%, a copper oxide concentrate with copper and cobalt grades of 10.16% and 0.56%, copper and cobalt recovery rates of 71.05% and 41.89%,a enhanced flotation concentrate with copper and cobalt grades of 1.41% and 0.21%, copper and cobalt recovery rates of 8.00% and 12.83% were obtained. The total copper recovery rate of copper sulfide concentrate, copper oxide concentrate and was 83.15%, and the total cobalt recovery rate was 62.55%. The resource utilization rate of high mud copper-cobalt ore is significantly im‐ proved.

Key words: high mud copper-cobalt ore, anionic collector RS, flotation