为提高云南某铜铅锌多金属矿的选矿指标,降低选矿药剂成本,提升经济效益,在矿石 性质研究的基础上,进行了铜铅混合浮选工艺试验研究。试验结果表明:在捕收剂丁基黄药+Z-200 用量为(50+30)g/t,锌抑制剂硫酸锌+亚硫酸钠用量为(600+300)g/t,起泡剂BK204用量为30 g/t,一段 磨矿细度为-0.074 mm80%,粗精矿再磨细度为-0.032 mm90%的条件下,经 1粗 2扫、1粗精再磨 2精 的铜铅混合浮选流程,可获得铜品位12.06%、铅品位18.85%、锌品位6.14%、铜回收率87.98%、铅回收 率85.33%、锌回收率4.22%的铜铅混合精矿。   

  1. 云南铜业股份有限公司矿山研究院
  • 出版日期:2024-03-18 发布日期:2024-08-16

Experimental Study on Copper-lead Mixed Flotation Process of a Polymetallic Ore in Yunnan

In order to improve the beneficiation index of a copper-lead-zinc polymetallic ore in Yun⁃ nan,reduce the cost of beneficiation reagents and improve economic benefits,based on the study of ore properties,an experimental study on copper-lead mixed flotation process was carried out.The results show that under the conditions of collector butyl xanthate + Z-200 dosage of(50 + 30)g/t,zinc inhibitor zinc sul⁃ fate + sodium sulfite dosage of(600 + 300)g/t,foaming agent BK204 dosage of 30 g/t,primary grinding fineness of -0.074 mm 80%,and coarse concentrate regrinding fineness of -0.032 mm 90%,the copper-lead mixed flotation process of one roughing-two scavenging-one roughing concentrate regrinding-two cleaning is carried out. The copper-lead mixed concentrate with copper grade of 12.06%,lead grade of 18.85%,zinc grade of 6.14%,copper recovery of 87.98%,lead recovery of 85.33% and zinc recovery of 4.22% can be obtained.   

  1. Mining Research Institute of Yunnan Copper Co.,Ltd.
  • Online:2024-03-18 Published:2024-08-16

摘要: 为提高云南某铜铅锌多金属矿的选矿指标,降低选矿药剂成本,提升经济效益,在矿石 性质研究的基础上,进行了铜铅混合浮选工艺试验研究。试验结果表明:在捕收剂丁基黄药+Z-200 用量为(50+30)g/t,锌抑制剂硫酸锌+亚硫酸钠用量为(600+300)g/t,起泡剂BK204用量为30 g/t,一段 磨矿细度为-0.074 mm80%,粗精矿再磨细度为-0.032 mm90%的条件下,经 1粗 2扫、1粗精再磨 2精 的铜铅混合浮选流程,可获得铜品位12.06%、铅品位18.85%、锌品位6.14%、铜回收率87.98%、铅回收 率85.33%、锌回收率4.22%的铜铅混合精矿。

关键词:

Abstract: In order to improve the beneficiation index of a copper-lead-zinc polymetallic ore in Yun⁃ nan,reduce the cost of beneficiation reagents and improve economic benefits,based on the study of ore properties,an experimental study on copper-lead mixed flotation process was carried out.The results show that under the conditions of collector butyl xanthate + Z-200 dosage of(50 + 30)g/t,zinc inhibitor zinc sul⁃ fate + sodium sulfite dosage of(600 + 300)g/t,foaming agent BK204 dosage of 30 g/t,primary grinding fineness of -0.074 mm 80%,and coarse concentrate regrinding fineness of -0.032 mm 90%,the copper-lead mixed flotation process of one roughing-two scavenging-one roughing concentrate regrinding-two cleaning is carried out. The copper-lead mixed concentrate with copper grade of 12.06%,lead grade of 18.85%,zinc grade of 6.14%,copper recovery of 87.98%,lead recovery of 85.33% and zinc recovery of 4.22% can be obtained.