预先分级联合选别提高某低品位铜矿金属回收率试验

罗增鑫   

  1. 紫金矿业集团股份有限公司
  • 出版日期:2020-03-25 发布日期:2021-09-13

Experiment on Improving the Metal Recovery of a Lowgrade Copper Ore by Preclassification Combined Beneficiation

Luo Zengxin   

  1. Zijin Mining Group Co.,Ltd.
  • Online:2020-03-25 Published:2021-09-13

摘要: 某大型低品位金铜矿山较高品位铜矿石选用浮选工艺进行富集,低品位铜矿石则利用生物堆浸工艺生产阴极铜,该矿山生物堆场随着堆高的增加,酸铁不断浸出、铜浸出率下降。针对该生物堆浸低品位铜矿石,采用预先分级、选冶联合工艺,并对原有堆浸工艺进行优化,2 mm筛上产品柱浸试验浸出率为75.22%,比原工艺流程浸出率提高了5.08个百分点,铁累积浸出率同比下降了2.75个百分点。-2 mm产品通过浮选工艺最终可获得含铜20.20%、回收率87.21%,伴生金品位3.6 g/t、金回收率58.74%,伴生银品位83.7 g/t、银回收率为68.28%的铜精矿,以及含硫47.12%,回收率33.00%的硫精矿。预先分级、选冶联合工艺铜综合回收率为79.55%,较原生物浸出工艺铜浸出率69.14%提高10.41个百分点,并伴生回收贵金属金、银及副产品硫精矿,使用该工艺可增加利润约1.16亿元。工艺改造后不仅可提高资源利用率,产生较大的经济效益,还可降低酸铁的浸出,大大降低环保处理成本。

关键词: 低品位铜矿 浸出率 资源利用 环保成本

Abstract: In a largescale lowgrade gold copper mine,the flotation process is used to enrich the highgrade copper ore,while the biological heap leaching process is used to produce cathode copper for the lowgrade copper ore.With the increase of the heap height,the leaching rate of iron in the mine keeps increasing,but the copper leaching rate decreasing.With regard to the biological heap leaching of lowgrade copper ore,the preclassification and smelting combined process was adopted,and the original heap leaching process was optimized.The leaching rate of the +2 mm sieve products in the column leaching test was 75.22%,which was 5.08 percentage points higher than the original leaching rate,and the iron cumulative leaching rate decreased by 2.75 percentage points.2 mm products can finally obtain copper concentrate containing 20.20% copper,with recovery rate of 87.21%,associated gold grade of 3.6 g/t,gold recovery rate of 5874%,associated silver grade of 83.7 g/t,silver recovery rate of 68.28%,and sulfur concentrate containing 47.12% sulfur with recovery rate of 33.00% through flotation process.So by using pregrading and metallurgy process,not only the comprehensive recovery rate of copper reaches 79.55% which is 10.41 percentage points higher than that of 69.14% by the original bioleaching process,but also get some associated gold,silver and sulfur concentrate.What's more,the new process will increases about RMB 116 million profits.In conclusion,the new process will bring a large number of benefits,including raising the utilization efficiency of resource,reducing the leaching of ferric acid,achieving remarkable economic benefit,and greatly saving the environmental protection cost.